TB 43-0213
TA504875
Figure 11-4. Rustproofing Stake Pockets.
b. Check wet film thickness with a wet film
of 10 mils is required. In areas where a wet film
thickness of 10 mils cannot be obtained or where
thickness cannot be measured, inspect for complete-
ness of coverage.
c. Check all drain holes to ensure that they are
open.
d. Check all inspection holes and drilled access
holes to ensure that compound coverage is adequate.
Use of a high intensity inspection light will enhance this
process.
e. Check vehicle to ensure that no compound has
been applied to prohibited areas (see CAUTION,
TA504789
Figure 11-5. Film Thickness Gage.
11-4